Národní úložiště šedé literatury Nalezeno 9 záznamů.  Hledání trvalo 0.01 vteřin. 
Measurement of surface tension for surface characterization of advanced ceramic materials
Mišáková, Liliana ; Kachlík, Martin (oponent) ; Salamon, David (vedoucí práce)
The presented thesis theoretically describes methods applied for the characterization of organic substances presented on the surfaces of advanced ceramic materials. Measurement of contact angles experimentally verifies the changes on surfaces of advanced ceramics. These changes are caused by the contamination of the surface. Adsorption of organic compounds on inorganic surfaces is rather unfavorable, therefore obtained results may provide useful information about the mechanisms of removal of the contaminants from surface. In the experimental part, water contact angle measurements were used to monitor and describe the changes of surface characteristics of ceramic oxides ZnO, TiO2, hydroxyapatite, Al2O3 and ZrO2. WCAs for untreated surfaces along with the WCA values for thermally or chemically treated surfaces of studied materials were assessed and compared in order to describe changes in surface energy, hydrophilicity and adhesivity caused by adsorbed organic adlayer. The decrease of contact angle values was achieved by cleaning of the surface with subsequent deprivation of adsorbed molecules.
Pohyb kapky po nakloněné rovině
Habr, Martin ; Jašíková, Darina (oponent) ; Fialová, Simona (vedoucí práce)
Práca sa zaoberá teóriou čiastočnej zmáčavosti steny, podľa ktorej je odvodený vzťah pre rýchlosť kvapky pohybujúcej sa po naklonenej rovine v závislosti na čase. V práci sú vysvetlené základné pojmy s touto teóriou súvisiace. Prostredníctvom rozboru divergencie normálového vektoru povrchu kvapky je vypracovaný postup matematického vyhodnotenia zložky dynamickej adhéznej sily. V rámci diplomovej práce bol vykonaný experiment, pri ktorom bola na štyroch analyzovaných povrchoch zisťovaná rýchlosť kvapiek rôznych objemov pri rozličných uhloch naklonenia roviny. Z výsledkov experimentu sú pomocou nelineárnej regresie vyhodnotené neznáme parametre, ako adhézny súčiniteľ, zložka dynamickej adhéznej sily a počiatočná a konečná rýchlosť kvapky. V rámci diplomovej práce bola vykonaná simulácia pohybu kvapky po naklonenej rovine v programe ANSYS Fluent. Záverom sú jednotlivé výsledky zhodnotené, porovnané a sú navrhnuté nové postupy, ktoré by mohli pomôcť pri ďalšom výskume stekania kvapky.
Studium vztahu mezi podmínkami testu FNCT (Full Notched Creep) a rychlostí šíření trhliny SCG (Slow Crack Growth) pro hodnocení odolnosti HDPE vůči růstu trhlin
Porubský, Tomáš ; Sadílek, Jiří (oponent) ; Petrůj, Jaroslav (vedoucí práce)
Teoretická časť predstavuje súhrn materiálových a testovacích parametrov ovplyvňujúcich priebeh SCG a následne aj dĺžku trvania FNCT testu. Experimentálna časť sa zameriava na modifikáciu podmienok FNCT testu s cieľom maximálneho zníženia času do lomu skúšaného materiálu. Pre vybrané 4 druhy tenzidov: Arkopal N110, Dodecylbenzénsulfonát sodný (NaDBS), Disponil LDBS55 a Simulsol SL8 boli uskutočnené FNCT testy. Najvýraznejší urýchľovací účinok bol pozorovaný u NaDBS, ktorý spôsobil viac než 2-násobnú redukciu času do lomu oproti referenčnému Arkopalu N110, pri rovnakej koncentrácii 11 % a podmienkach testu FNCT: 50 °C, 9,0 MPa. Urýchľovací účinok NaDBS bol porovnaný pre 2 polyethylénové materiály: Liten VB85 a VL 20N. Pri podmienkach testu 80 °C a 4 MPa bolo 5% roztokom NaDBS spôsobené takmer 12,5-násobné urýchlenie oproti konvenčnému 2% Arkopalu N110 pre VL 20N a skoro 8,5-násobné pre VB 85. Bola objavená závislosť medzi schopnosťou tenzidu zmáčať študovaný materiál a FNCT časom do lomu.
Povrchové úpravy biomateriálů v dielektrickém bariérovém výboji
Maruniak, Marek ; Přikryl, Radek (oponent) ; Mazánková, Věra (vedoucí práce)
Práca sa zaoberá opracovaním povrchov rôznych polymérnych biomateriálov pomocou plazmy generovanej za atmosférického tlaku. Plazma je generovaná medzi dvoma elektródami pričom medzi nimi je vložené dielektrikum. Za použitia tohto typu výboja sa skúma zmena povrchových vlastností opracovaného materiálu ako je povrchová energia a kontaktný uhol v závislosti na dobe opracovania. Vyhodnotenie výsledkov povrchovej analýzy bolo uskutočnené metódou merania kontaktného uhlu a povrchovej energie pomocou prístroja See System. Cieľom práce bolo porovnať zmenu povrchových vlastností materiálu pred opracovaním a po opracovaní v plazme ako aj zmenu povrchových vlastností v závislosti na dobe starnutia. Výsledky sa líšia od typu použitého materiálu.
Measurement of surface tension for surface characterization of advanced ceramic materials
Mišáková, Liliana ; Kachlík, Martin (oponent) ; Salamon, David (vedoucí práce)
The presented thesis theoretically describes methods applied for the characterization of organic substances presented on the surfaces of advanced ceramic materials. Measurement of contact angles experimentally verifies the changes on surfaces of advanced ceramics. These changes are caused by the contamination of the surface. Adsorption of organic compounds on inorganic surfaces is rather unfavorable, therefore obtained results may provide useful information about the mechanisms of removal of the contaminants from surface. In the experimental part, water contact angle measurements were used to monitor and describe the changes of surface characteristics of ceramic oxides ZnO, TiO2, hydroxyapatite, Al2O3 and ZrO2. WCAs for untreated surfaces along with the WCA values for thermally or chemically treated surfaces of studied materials were assessed and compared in order to describe changes in surface energy, hydrophilicity and adhesivity caused by adsorbed organic adlayer. The decrease of contact angle values was achieved by cleaning of the surface with subsequent deprivation of adsorbed molecules.
Drop coating deposition Raman spectroscopy of biologically important molecules
Kuižová, Alžbeta ; Kočišová, Eva (vedoucí práce) ; Holoubek, Aleš (oponent)
Ramanova spektroskopie kapkově nanášených povlaků (DCDR) je speciální metodou Ramanovy spektroskopie, která je založená na zasychání kapek roztoku nebo suspenze na hydrofóbním substrátu, co ve většině případů vede k tvorbě prstence známého jako "kávový kroužek". Výsledkem je zakoncentrování materiálu a vyšší intenzita Ramanova signálu ve srovnání s Ramanovym rozptylem z roztoku. V práci byly porovnány substráty s různou drsností a hydrofobicitou: hladký substrát s vrstvou polytetrafluoretylenu (pPTFE) a nanodrsné substráty, kde byla hydrofobicita povrchu zvýšená nadeponovanými měděnými nebo stříbrnými nanočásticemi s různou koncentrací. Pro suspenzi liposomů z lipidu DPPC docházelo k lepšímu zakoncentrování v případe substrátů s vyšším kontaktním uhlem, kde je vyšší hydrofobicita dosáhnuta nanodrsným povrchem. Mezi jednotlivými zdrsněnými substráty k výraznému zlepšení nedocházelo. V případě schnutí kapek při různých teplotách (v rozsahu od 15 do 60řC) nanesených na hladký pPTFE substrát a povrch s nadeponovanými stříbrnými nanočásticemi, Ramanova spektra neukázala spektrální změny souvisící s fázovým přechodem lipidů. Pro teploty zasychání vyšší než teplota fázového přechodu byly na vzniklých prstencích pozorovány nehomogenity, které při teplotě 45řC vedly k vyššímu Ramanovu signálu. Závěrem, k lepšímu...
Povrchové úpravy biomateriálů v dielektrickém bariérovém výboji
Maruniak, Marek ; Přikryl, Radek (oponent) ; Mazánková, Věra (vedoucí práce)
Práca sa zaoberá opracovaním povrchov rôznych polymérnych biomateriálov pomocou plazmy generovanej za atmosférického tlaku. Plazma je generovaná medzi dvoma elektródami pričom medzi nimi je vložené dielektrikum. Za použitia tohto typu výboja sa skúma zmena povrchových vlastností opracovaného materiálu ako je povrchová energia a kontaktný uhol v závislosti na dobe opracovania. Vyhodnotenie výsledkov povrchovej analýzy bolo uskutočnené metódou merania kontaktného uhlu a povrchovej energie pomocou prístroja See System. Cieľom práce bolo porovnať zmenu povrchových vlastností materiálu pred opracovaním a po opracovaní v plazme ako aj zmenu povrchových vlastností v závislosti na dobe starnutia. Výsledky sa líšia od typu použitého materiálu.
Pohyb kapky po nakloněné rovině
Habr, Martin ; Jašíková, Darina (oponent) ; Fialová, Simona (vedoucí práce)
Práca sa zaoberá teóriou čiastočnej zmáčavosti steny, podľa ktorej je odvodený vzťah pre rýchlosť kvapky pohybujúcej sa po naklonenej rovine v závislosti na čase. V práci sú vysvetlené základné pojmy s touto teóriou súvisiace. Prostredníctvom rozboru divergencie normálového vektoru povrchu kvapky je vypracovaný postup matematického vyhodnotenia zložky dynamickej adhéznej sily. V rámci diplomovej práce bol vykonaný experiment, pri ktorom bola na štyroch analyzovaných povrchoch zisťovaná rýchlosť kvapiek rôznych objemov pri rozličných uhloch naklonenia roviny. Z výsledkov experimentu sú pomocou nelineárnej regresie vyhodnotené neznáme parametre, ako adhézny súčiniteľ, zložka dynamickej adhéznej sily a počiatočná a konečná rýchlosť kvapky. V rámci diplomovej práce bola vykonaná simulácia pohybu kvapky po naklonenej rovine v programe ANSYS Fluent. Záverom sú jednotlivé výsledky zhodnotené, porovnané a sú navrhnuté nové postupy, ktoré by mohli pomôcť pri ďalšom výskume stekania kvapky.
Studium vztahu mezi podmínkami testu FNCT (Full Notched Creep) a rychlostí šíření trhliny SCG (Slow Crack Growth) pro hodnocení odolnosti HDPE vůči růstu trhlin
Porubský, Tomáš ; Sadílek, Jiří (oponent) ; Petrůj, Jaroslav (vedoucí práce)
Teoretická časť predstavuje súhrn materiálových a testovacích parametrov ovplyvňujúcich priebeh SCG a následne aj dĺžku trvania FNCT testu. Experimentálna časť sa zameriava na modifikáciu podmienok FNCT testu s cieľom maximálneho zníženia času do lomu skúšaného materiálu. Pre vybrané 4 druhy tenzidov: Arkopal N110, Dodecylbenzénsulfonát sodný (NaDBS), Disponil LDBS55 a Simulsol SL8 boli uskutočnené FNCT testy. Najvýraznejší urýchľovací účinok bol pozorovaný u NaDBS, ktorý spôsobil viac než 2-násobnú redukciu času do lomu oproti referenčnému Arkopalu N110, pri rovnakej koncentrácii 11 % a podmienkach testu FNCT: 50 °C, 9,0 MPa. Urýchľovací účinok NaDBS bol porovnaný pre 2 polyethylénové materiály: Liten VB85 a VL 20N. Pri podmienkach testu 80 °C a 4 MPa bolo 5% roztokom NaDBS spôsobené takmer 12,5-násobné urýchlenie oproti konvenčnému 2% Arkopalu N110 pre VL 20N a skoro 8,5-násobné pre VB 85. Bola objavená závislosť medzi schopnosťou tenzidu zmáčať študovaný materiál a FNCT časom do lomu.

Chcete být upozorněni, pokud se objeví nové záznamy odpovídající tomuto dotazu?
Přihlásit se k odběru RSS.